- - By SKY59 Date 03-24-2006 15:33
Looking for some advice on best methods of welding clad plate.
The material is 5/16" A36 Carbon Steel clad to 3/32" B575 C276 Hastalloy
We are using GMAW in DCEP pulsed mode with Lincoln .035" 686 CPT wire.Shield gas is 90He10Ar for welding from A36 side and 90Ar10He for
welding on Hastalloy side. Any suggestions for shield gas or wire to
obtain best results?



Parent - By Bill M (***) Date 03-24-2006 17:04
Do you have a copy of the hastalloy alloy product brochure?

It has lots of welding info and is available for downloading as a .pdf file at:

www.haynesintl.com/mini/C22s/C22.htm