- - By Chris Martin (*) Date 03-27-2006 13:11
Hello everyone,

I have a small pure molly project coming up and I need some advice on technique. I will be welding .250" and .3750" pure molly rods together to make something that looks similar to a bird cage. I will be welding it in a glove box. Are there any special techniques to welding this material together?

Thanks for your help.

Chris
Parent - By jwright650 (*****) Date 03-27-2006 15:39
Do you know the ASTM number of the material you are working with? This info may help others give a better answer to your question.
John Wright
Parent - By Chris Martin (*) Date 03-27-2006 17:08
Not sure of the ASTM # is but it's 99.9% pure.