why cross joint is not permitted ? I mean that if two weld seams meet together in cross joint or in pluse joint shape what is the reason of preventing of this kind of joint?
I'm not sure what you mean by cross joint or pulse joint. If you're referring to tying welds together that are on opposite sides of a common plane, they are not tied together because of the potential for notching.