- - By dschlotz (***) Date 05-27-2006 12:12
I like the feel of the expensive welding gloves but not the price. I have learned a new trick. I save my old gloves that are usually worn out on only one side. When I wear a hole in a new pair, I cut a finger off of the old and cover the whole finger of my newer glove. I use spray adheasive to keep my patch in place. It extends the life of gloves buy at least 5 times for me. 

Dennis
Parent - By texredneck (**) Date 05-31-2006 16:54
Great Idea thanks!
Parent - By scrapiron Date 06-11-2006 10:48
that is a neat trick-I work in a scrap yard-so l get plenty of free used welding  gloves l can repair-and use for burning-thanks