To secure reprints of Inspection Trends contact the American Welding Society at 800-443-9353 or email


Welding Metallurgy, Part 1: Understanding Mechanical Properties · Eddy Current Testing of Partly Magnetic Stainless Steels · NDE Helps Extend the Life of Paper Mill Steam Drums

Selecting a Nondestructive Testing Method: Visual Inspection · Ensuring Vessel Integrity with Acoustic Emission Testing ·
Welding Metallurgy, Part 2: Physical Properties

Inspecting Rail Tank Cars · Welding Metallurgy, Part Three: The Inspection Process · The Facts about CWI Endorsements
· Meeting the Challenges of Digital Radiography

Long-Range Guided-Wave Ultrasonics: A New Age in Pipeline Inspection
· The Changing Roles of Inspectors · Selecting a Nondestructive Testing Method: Eddy Current Testing · Eight Things You Should Know about Leak Testing Equipment · Using Eddy Current for Corrosion Inspection