FLAT STORAGE HOIST RING
- Forged Alloy Steel - Heat
Treated - Black Oxide Finish - Pivots 180° - 6:1 Safety
Factor Important Note: To achieve maximum load strength, High
Strength Socket Head Screws must be used (P/N's 470-60 thru
470-62). (Mounting screw not included) |

|
HIGH STRENGTH SOCKET HEAD SCREW |
|
HEAVY DUTY HOIST RING
- Heavy Duty - Load Rating to 12,000
lbs.* - Swivel 360° - Pivots 180° - 5:1 Safety
Factor TECHNICAL INFORMATION MATERIAL: 4140 Aircraft quality
high strength alloy steel with minimum tensile strength of 180,000
psi, certified heat treatment with 100% magnaflux inspection.
Corrosion resistant plating. Maximum operating temperature: 400°
F. * For load ranges of 15,000 to 1000,000 lbs. call All American
for price and availability. |

|
HOIST RING ASSEMBLIES
- STANDARD CLEVIS
- LONG CLEVIS
- Safety Engineered - Swivel 360° -
Pivots 180° - 5:1 Safety Factor - Replaces Conventional
eyebolts TECHNICAL INFORMATION MATERIAL:4140 High strength
alloy steel. FINISH:Black Oxide Clevis,bolt, pins and bushing
are magnetic particle inspected. * Stated load capacity based on
specific thread torques as shown in the table. ** It is
recommended that these torques be used when installing hoist
rings. |

|
SIDE
PULL HOIST RINGS
- STANDARD SIZES
- METRIC SIZES
- Side-Pull Feature - Extra Large
Rings - 5:1 Safety Factor TECHNICAL INFORMATION MATERIAL:
High strength alloy steel. Clevis, ring, bushing and cap screw
are magnetic particle inspected. Clevis is x-rayed. The swivel
and pivot action of the Side-Pull Hoist Ring allows you to flip and
turn parts without unhooking. You are also able to use almost any
size hook because of the extra large diameter rings. * Stated
load capacity based on specific thread torques as shown in the
table. ** It is recommended that these torques be used when
installing hoist rings. |

|
METRIC HOIST RING ASSEMBLIES
-Safety
Engineered -Swivel 360° -Pivots 180° -5:1 Safety
Factor -Replaces Conventional Eye
Bolts
TECHNICAL INFORMATION -MATERIAL: 4140 High strength alloy
steel. -FINISH: Black Oxide -Clevis, bolt, pins and bushing
are magnetic particle inspected. |

|
HEAVY
DUTY SAFETY HOIST RINGS Heavy Duty
Swivel 360°
Pivots 180°
5:1 Safety Factor
TECHNICAL INFORMATION
MATERIAL: 4140 Aircraft quality high strength
alloy steel with minimum tensile strength of
180,000 psi., certified heat treatment with
100% magnaflux inspection.
Corrosion resistant plating.
Maximum operating temperature: 400° F. |

|
WELDLESS
ALLOY RINGS NEW!
NOTE: Minimum ultimate load is 6 times the working load
limit. Rings meet Federal Specification RR-C 271D, Type VI
|

|
BOLT
TYPE ANCHOR SHACKLE NEW!
NOTE: Minimum ultimate load is 6 times the working load
limit. Bolt type anchor shackles supplied with thin head bolt
& nut with cotter pin. Meet Federal Specification RR-C 271D,
Type IVA, Grade A, Class 3 |

|
SUPER
COIL™ HOIST RINGS NEW!
- Alloy Steel, Black Oxide Finish
- Standard coil thread sizes from
3/4" to 1-1/2"
- Excellent for temporary attachment
to steel & construction material
- Range of movement: pivot 180° &
swivel 360° to compensate for
pitch, pull and sway when lifting
unbalanced loads. Load ratings
are for lifts in any direction
- MINIMUM SAFETY FACTOR = 5:1
- Meets OSHA standards
- 100% Magnetic Particle Inspected
- Destructive testing by outside
independent laboratories
- COIL BOLTS are included to ensure
the integrity of the product
|

|
HEAVY
DUTY STEEL PLATE HOIST RING NEW!- Pivots 180°/Swivels 360°
- Material: Forged alloy steel
- Minimum tensile strength of 180,000 psi
- 100% Magnetic Particle Inspected
- Safety Factor: 5:1
- Finish: Black Oxide per Mil C-13924B
(Cadmium plated available)
|

|
HEAVY
DUTY WELD-MOUNT HOIST RING NEW!
- Pivots 180°/Swivels 360°
- Material: Forged alloy steel
- Minimum tensile strength of 180,000 psi
- 100% Magnetic Particle Inspected
- Safety Factor: 5:1
- Finish: Black Oxide per Mil C-13924B
(Cadmium plated available) |

|
UNIVERSAL
LIFT RINGS NEW!
Some typical applications for the American Arialal lift rings
are: 1. Large Chucks
2. Milling Cutters
3. Dies
4. Broaches
5. Motors
6. Fixtures
7. Small Machines
8. Machined parts AMERICAN’S ArialAL LIFT RING PROVIDES SIX
COMMONLY USED THREAD SIZES (1/4-20, 5/16-18, 3/8-16, 1/2-13,5/8-11
AND 3/4-10). |

|
HEAVY
DUTY PIVOT LIFT PLATE HOIST RING NEW!
Some typical applications for the American Arialal lift rings
are: - Pivots 180°
- Material: Forged alloy steel
- Minimum tensile strength of 180,000 psi
- 100% Magnetic Particle Inspected
- Safety Factor: 5:1
- Finish: Black Oxide per Mil C-13924B
(Cadmium plated available) |

|
AA’S NEW & IMPROVED
PATENTED HEAVY DUTY SIDE-PULL HOIST RINGS

UP TO 40% STRONGER
The BEST
VALUE and STRONGEST side-pull hoist ring
available.
AA’s UNIQUE new hoist ring is FULLY
RATED at 5:1 in VERTICAL as well as conventional
SIDE-PULL and has the highest load rating for a given
mounting screw size of any other side-pull ring
available
This new patented design stays in one piece
even when not threaded into the workpiece
NO LOOSE PARTS THAT CAN BE LOST!!!
PLEASE SEE BELOW
|
HEAVY DUTY
SIDE-PULL HOIST RING NEW!
- Self-aligning in the direction of the load
- Rotates 360°
- Minimum of 5:1 safety factor in any direction
- Unit is supplied in one (1) piece so
that parts cannot get lost
- Alloy steel, black oxide finish
- 100% magnetic particle inspected
|

|
SWIVEL EYEBOLT
TAMPER RESISTANT DESIGN NEW!
The Jergens Swivel Eyebolt™ lifting product has a full swivel and
pivoting action which allows for the flipping and turning of the
part without unhooking. The patented tamper resistant design is
ideal for permanent mounting on OEM applkications or on molds, dies
and fixtures. - Tamper Resistant Design
- Swivels 360°, Pivots 180°
- Eliminates Bending (of Eyebolt) Problem
- Forged, Oversized, One-Piece Lift Ring
- Rated at 5:1 Strength Factor
- Load Capacities to 4000 Lbs / 2000 Kg
- Economically Priced
- Material: Alloy Steel, or 316 Stainless Steel
- Finish: Black Oxide, or Passivated (SS)
|

U.S. Patent #5634734 Foreign Patent Pending |
SWIVEL
EYEBOLT INSTALLATION TOOL NEW!
|

|
FORGED
CENTER PULL NEW!
- STANDARD SIZES
- METRIC SIZES
Forged Center Pull Hoist Ring integrates a solid center brace
lift bail into our most popular style product. This design
eliminates the possibility of spreading the lift ring in
misapplications. Forged hoist rings are ideal for OEM and industrial
use. - Tamper Resistant Design
- Full (over center) swivel and pivot action
- Capacities up to 5000 Ibs
- 5:1 strength factor-alloy steel
- Made in U.S.A.
|

|
SIDE
SWIVEL™ NEW!
- STANDARD SIZES
- METRIC SIZES
Side Swivel™ Lifting Ring is designed specifically for OEM type
applications. It replaces potentially dangerous eyebolts on
commercial, military, and industrial lifts requiring full swivel and
pivoting action. - Tamper Resistant Design
- 51 strength factor-forged ring
- Unique 3 piece design
- Capacities up to 4100 Ibs.
- Made in U.S.A.
|

|