Technical Standards Notic...

AWS TECHNICAL STANDARDS NOTICES


NEW STANDARDS PROJECTS
Development work has begun on the following new or revised standards. Directly and materially affected individuals are invited to contribute to the development of such standards. Those wanting to participate may contact the Staff Engineer listed with the document.

Participation on AWS Technical Committees and Subcommittees is open to all persons.

A5.2/A5.2M:201X, Specification for Carbon and Low-Alloy Steel Rods for Oxyfuel Gas Welding.
This specification prescribes requirements for the classification of carbon and low-alloy steel rods for oxyfuel gas welding.

  • Stakeholders: Welding schools, welding professionals, fabricators and construction companies
  • Revised Standard
  • Staff Contact: R. Gupta, x301

A5.10/A5.10M:2012 (ISO 18273:2004 MOD), Welding Consumables–Wire Electrodes, Wires and Rods for Welding of Aluminum and Aluminum-Alloys – Classification.
This standard specifies requirements for classification of solid wires and rods for fusion welding of aluminum and aluminum alloys. The classification of the solid wires and rods is based on their chemical composition.

  • Stakeholders: Welding professionals, fabricators and construction companies
  • Revised Standard
  • Staff Contact: R. Gupta, x301

A5.14/A5.14M:201X (ISO 18274:2010 MOD), Welding Consumables – Solid Wire Electrodes, Solid Strip Electrodes, Solid Wires and Solid Rods for Fusion Welding of Nickel and Nickel-Alloys – Classification.
This standard specifies requirements for classification of solid wire electrodes, solid strip electrodes, solid wires and solid rods for fusion welding of nickel and nickel alloys. The classification of the solid wire electrodes, solid strip electrodes, solid wires and solid rods is based on their chemical composition.

  • Stakeholders: Welding schools, welding professionals, fabricators and construction companies
  • Revised Standard
  • Staff Contact: R. Gupta, x301

 


STANDARDS FOR PUBLIC REVIEW

AWS was approved as an accredited standards-preparing organization by the American National Standards Institute (ANSI) in 1979. AWS rules, as approved by ANSI, require that all standards be open to public review for comment during the approval process. This column also advises of ANSI approval of documents. The standards listed below are under public review. A draft copy may be obtained through the AWS staff contact for the respective standard. Send correspondence to AWS, Technical Services Division, 8669 NW 36 Street, #130, Miami, FL 33166; telephone (800/305) 443-9353.

B2.1-1/8-231:201X, Standard Welding Procedure Specification (SWPS) for Gas Tungsten Arc Welding with Consumable Insert Root followed by Shielded Metal Arc Welding of Carbon Steel (M-1/P-1, Groups 1 or 2) to Austenitic Stainless Steel (M-8/P-8, Group 1), 1/8 inch [3 mm] through 1-1/2 inch [38 mm] Thick, IN309, ER309, and E309-15, -16, or -17, or IN309, E309(L), and E309(L)-15, -16, or -17, in the As-Welded Condition, Primarily Pipe Applications
Revised Standard – $124.00 [ANSI Public Review expires 7/13/15]
Staff Contact: J. Rosario, ext. 308

D1.5M/D1.5:2015, Bridge Welding Code
Revised Standard – $176.00 [ANSI Public Review expires 7/13/15]
Staff Contact: S. Borrero, ext. 334

 


ISO DRAFT STANDARDS FOR PUBLIC REVIEW
Copies of the following Draft International Standards are available for review and comment through your national standards body, which in the United States is ANSI, 25 West 43rd Street, Fourth Floor, New York, NY, 10036; telephone (212) 642-4900. Any comments regarding ISO documents should be sent to your national standards body.

In the United States, if you wish to participate in the development of International Standards for welding, contact Andrew Davis at AWS, 8669 NW 36 Street, #130, Miami, FL, 33166; telephone (305) 443-9353 ext. 466, e-mail: adavis@aws.org. Otherwise contact your national standards body.

None at this time.

 


NEW STANDARDS APPROVED BY ANSI:
None at this time.

 


REVISED STANDARDS APPROVED BY ANSI:

None at this time.

 


REAFFIRMED STANDARDS APPROVED BY ANSI:
None at this time.

 


WITHDRAWN STANDARDS APPROVED BY ANSI:
None at this time.

 


AMENDMENT STANDARDS APPROVED BY ANSI:
None at this time.

 


ADDENDA STANDARDS APPROVED BY ANSI:
None at this time.