9.1 shet metal welding code and 1.3 strucural welding code - sheet metal seem very similar in title and description
as far as I can tell 1.3 has arc spot and arc seam, and 9.1 has brazing information? I've been designing light guage SS 304 and mild steel sheet from 11-20 guage (mostly 16-20) and I was wondering which would have more useful design information. Only process we use is GTAW and GMAW so I'm not too keen about arc spot or brazing. We have both structural and non structural joints, currently I'm using D1.6 but that only covers material down to 1/4" or 1/8" so I'm wondering if these codes would have any useful design information or joint configurations I could reference?
I'm not actually welding to code, but I've been designing and detailing joints off of the D code as that seems like a smart idea
any clarification about what they contain?