Tin (molecular mass 118.7, specific gravity 7.28, melting point 231.9 degrees Centigrades), is a metal that belongs to the same chemical family than lead and germanium.
Apart from soldering, it's widely used for making copper alloys (bronze for example), and for surface protection of some metals (steel for example).
Giovanni S. Crisi
Sao Paulo - Brazil