No, a square groove joint is just 2 pieces butted straight up, no joint prep at all. It is still considered a groove weld, hense the name "square groove". If you are grinding all the weld off flush with the base material afterwards, then it becomes a flush butt joint. You only get thrown into 4.19.3 category if you are grinding the weld flush after welding. If your not, then you go by clause 4.19.2 which allows 3/32" weld reinforcement because you are welding a sqaure groove joint. Hope this helps and if not, speek up. We might not be on the same page yet.;-)