By broberts13
Date 06-23-2008 01:32
Edited 06-23-2008 01:46
I can't seem to get a good weld on an inside corner (T weld). I need to weld a 1" square bar to 1/4" plate and 1/4" wall square tube to 1/2" plate.
Using a stick welder, and 1/8", 6011 and 6013 rods, I get what my book calls poor fusion. It looks like a bead on each piece with a void between the 2 beads. I've tried currents from 70A to 160A with the same results. I can lay a beautiful bead on a flat piece of the same material at a wide range of currents. I get a good inside bead from my 120A flux core wire feed welder, but I don't think it has the penetration I need.