Don't whip the low hydrogen elecrode as you would with a cellulose covered electrode such as E6010 or E7010 while making the root pass.
Hold a short arc, use a slight "whip", but keep the electrode in the molten puddle such that you move to the leading edge of the puddle and then back to the trailing edge of the puddle.
Best regards - Al