- - By Naturaledge Date 07-20-2008 17:34
I am making boxes out of stainless mesh and want to weld them along one side and bottom . thank you
Parent - By JAYDESAI (*) Date 07-21-2008 03:44
Hope you are deploying Spot Welder in this !
Parent - By Metarinka (****) Date 07-21-2008 13:25
You didn't really ask a quesiton... As mentioned resistance spot welding would be the easiest. It could be tig welded, but you'll run into trouble due to it being a mesh.