- - By El Cazador (*) Date 08-08-2008 02:39
Just getting started with tig.  Looking to buy a 25' water cooled torch.  Weldcraft I guess since I tend to stick with what Miller has as I've had good luck with what I've got from Miller so far.  Any suggestions on where to go to get the best price?  And what model is the best fit for a Miller 180?
Thanks for any input.
Vic
Redlands, CA
Parent - By DaveBoyer (*****) Date 08-08-2008 03:13
    A #20 torch is easy to get consumables for, and about the right amperage range. The Weldcraft is actually a copy of an old Linde part, plenty of others make copies of it too.