With many manufacturers the 65 and 70 are the exact same stuff. Its economically efficient. They are poured from the same heats, run through the same heat treat, and tested with the same testing procedures. If the resulting mechanicals overlap both specs they will be dual certed.
In fact triple cert materials 60/65/70 are not that uncommon.