yea, we have a couple other procedures also, like the fabshield hot pass, but we dont have a repaire procedure for that so any repair will be a cutout. we also have 9018 hot,fill and cap, and we have a uphill fluxcored using 75/25. im really starting to like the fabshield, we put a 750 wall in the clamps at 8:00 saturday, the foreman said soon as were done were going to the house, at 10:45 we were off the ROW, i sure dont think i can do that with 70+