- - By Gregory Walker (*) Date 09-04-2008 00:17
Ok, my machine is not arcing at all it also has no auxillary power or it has a little it will spin my grinder about as fast as my daughters turtle runs.  Ive tried to excite it with a battery charger. I got the trouble shootn guides and it says you can excite it from a storage battery or another generator.  Could it be a wire or something I havent a clue any and all help is needed please.
Parent - By jaureweld (*) Date 09-04-2008 00:19
i had a 79 model lincoln the prob with mine not arcing was the shunt coils
Parent - - By snuffman (***) Date 09-04-2008 00:40 Edited 09-04-2008 00:42
[deleted]
Parent - - By Gregory Walker (*) Date 09-06-2008 15:51
I have another question and that is what do i excite this machine with.  Battery charger or another generator or can i use a little cracker jack box?
Parent - By Gregory Walker (*) Date 09-07-2008 18:08
thank you I got it welding this morning i excited it and got it going.