- - By vantage500man (**) Date 09-07-2008 23:40
Bought a 500 vantage 15 mouths ago and got it with a Cummins 3.3. I looked on Lincoln site at the vantage welders and now see no Cummins engines offered at all this sucks!
Any one know why Lincoln dropped the cummins engine line out of the vantage series
Parent - By SMTatham (**) Date 09-08-2008 13:51
This is due to Lincoln needing to use engines in the USA that meet EPA Tier 4i requirements for emissions. Cummins is still used on the export AirVantage; not sure about the export Vantage 500.