Reference: AWS D1.1 Table 4.1 - PQR done in 3G (plate) could only qualify Vertical position in production welding.
Case: Supporting PQR is done in 3G position. The contractor would like to support this for WPS which the contractor intend to qualify it(WPS) for ALL position. The contractor proposed to accept the WPS (all position) with PQR in 3G only with a suggestion that the qualification of welder will be done in 2G, 3G and 4G position.
Can this proposal be acceptable?