- - By SammyShine (**) Date 10-01-2008 23:17
I completed a PQR. The company I sent it to said some things were incorrect.

1. Is MIG welding Manual or Semi-Automatic? I marked Semi-Auto - they say Manual

2. Base Metal Material Spec is A36......My form has Material Spec __A36____ to ___(?)___
                                                                      Type or Grade ___50____ to __(?)____    They put a question mark on the second line

                                                                        
                                                                    
I thought the PQR would only state actuals not variances?
                                                                                      Thanks!
Parent - - By shipfitter88 (*) Date 10-02-2008 00:03
The Semi-automatic part should be correct and as far as the A-36 to ? it should have been A-36 to A-36 and the same for Type or Grade it's just stating you welded base metal A-36 to A-36.
Parent - By SammyShine (**) Date 10-02-2008 00:49
Thank you so much..that makes perfect sense.