Hello harl, if I'm following you correctly here you are saying that when you hook your LN 25 up to the machine in the CC mode that you see 40 volts on the volt meter and you think this means something is wrong? If this is what you are seeing while hooked up this way it is normal. It is likely that if you start welding with the LN 25 you will note a voltage drop that will be based on the amperage setting that you have set on the machine. I don't do a lot of welding with LN 25's on CV capable machines so I can't remember the exact difference there, however it is possible that you will see the actual voltage from the Big 40, as it is set, when using the CV tap. The main difference between the CC output and the CV tap output should be that the CC output will start out with maximum open circuit voltage and then drop to actual welding voltage upon welding start-up, whereas CV voltage will be determined by the setting on the machine and will remain relatively constant even after welding has been initiated. Hope this somewhat explains what you are seeing if I have understood your post correctly. Best regards, aevald
I cannot say for sure, not knowing exactly what model of Big 40 you have & the actual serial #, but the technical manual troubleshooting guide refers to possible PC 1 malfunction. Miller is usually very vague when it comes to board problems & in the case of this machine the main control board is hermetically sealed in a protective box Miller refers to as "the Vault" There is an LED board (PC 9) that will give indication as to whether the PC 1 board is functioning correctly. There is a series of LED sequences you can use to troubleshoot PC1 in a very general sense. Your owner's manual should have a sequence guide to follow.
I took this info from a Big 40 CAT diesel manual. There are several variations of machine & engines, I am assuming the electronics for late model machines will be basically the same. I could be mistaken though. It sounds as though you have a signal issue & I didn't see anything pertaining to a "memory" when using a remotely operated device. I take it you are connecting the LN 25 to the terminals on your machine & setting the BIG 40 to VS wire feeder, remote 14 switch OFF (or panel control) the contactor, being on & the lines "HOT". You set the coarse A/V range switch to the desired setting & set the fine adjustment as well. This machine, if I am looking at one similar to yours, only has two output terminals for weld current, not a separate set for CC & CV. It sounds like a control signal issue to me & I again, may be mistaken, but the machine electronically connects to CC & CV, not physically, like with a knife switch, or a separate set of terminals.
I would check PC 9 out & see if you have an obvious problem linked directly to the main control board. It seems odd, that if you spin the selector switch, it will start doing what it's supposed to. Something may have malfunctioned with that switch, or another control function when your buddy hooked his suitcase up to it using the remote 14 out. I can't say doing what you are now is going to fry something. As a rule, switching polarity, or TAP style range selector switches while under load will cause arcing & is very bad for them. Not recommended. The switch you are using is electronically controlling the weld selections & process options. That's probably where the problem's coming from. Wherever the switch is sending a signal to. I'm believing it to be PC 1. I hope this helps you out. If you take it to service, they will give you a better idea. If the PC 1 board is bad, I can direct you to a couple places that repair them for much less the cost of a new one.
Good luck. S.W.
One other thing you can do, is call the factory & ask for Performance Engine Drive division. Don't waste your time with the sales guys at your LWS, unless they know their stuff & know it well. John is REALLY good in PED & has walked me thru a few problems. I have a toll free number for them, PM me & I'll give it to you. This is for dealers & service techs ONLY, so I do not like to post it.
I believe your machine is using solid state electronics to create CV current, unlike a true CV machine with a separate tap or transformer windings you physically connect to. The problem most likely lies somewhere in that area, or in the control signal activating it. Again, I may be wrong. I have never worked on this machine & have no real familiarity with it. :-)
Good luck. Steve.