- - By doyenofcastle (**) Date 09-28-2008 13:37
which electrode better in E7018 Lincolin or Esab .we have offer in my company and Lincolin less than by 20 D,I knew I should make test for the electrode but also we can ask the experts people.I will use it in structure for rigs
Parent - - By freewelder (*) Date 10-15-2008 08:28 Edited 10-22-2008 03:45
This looks like it is in the wrong forum but we use neither. Kobelco works well.
Parent - - By TRC (***) Date 10-15-2008 21:59
Hey FW, where do you buy the Kebelco from?
Parent - By freewelder (*) Date 10-22-2008 03:48
Hi TRC, the link to Kobelco can be found on the front page of AWS home site; http://www.aws.org/w/a/index.html?id=UrjmHqYS
Parent - By millerman (**) Date 10-22-2008 18:13
i like the new 7018 excaliber from lincoln
Mac
Parent - - By TimGary (****) Date 10-22-2008 19:58
Both work very well, and I have not burned both manufacturers rods in the same day since 1997, but, I used to think that the ESAB Atom ARC 7018 rods left slag that was easier to remove than the Lincoln.

Tim
Parent - - By Cactusthewelder (*****) Date 10-22-2008 20:29
We all burn Lincoln 7018 Excaliber They work GREAT ! Slag peels easy.
Parent - By fbrieden (***) Date 10-22-2008 21:09
Lincoln LH-78. Just be careful with overhead, the slag just falls off the weld!