I'll update this for y'all...since no answers were forthcoming, my engineer and I explored the latest copy of the spec (keep in mind this spec was cancelled and not replaced in the 90s), and came up with class 1 for plating thickness of .00050" min. After discussing the requirement with the drawing's owners, it would appear that there was once a lazy detailer out there in aerospace land...:)