IF I WANT TO USE S275JR (EN 10025) STRUCTURAL STEEL PLATE WHICH GROUP IS APPLICABLE FOR THIS IN TABLE 3.2 OF D1.1
By
Noel Tan
Date
09-26-2008 03:55
This Material is considered unlisted material as per AWS D1.1, thus, it cannot be grouped.
Regards,
Noel Tan
By
Bka
Date
10-23-2008 17:08
qaqcmpm,
The S275RJ is out of AWS group. However you can convert to AWS material equivalent which is listed in AWS D1.1 table 3.1
S275RJ is equivalent ASTM A573 Gr 65. as per AWS D1.1 table 3.1 the ASTM A573 Gr 65 belong to AWS group I.
so S275RJ belong to AWS group I.
By
Noel Tan
Date
10-28-2008 08:43
Bka,
I always having problem to group BS steel in AWS Group according to table 3.1
Everytime i did that always commented and rejected by client.
Does this so called "equivalent" recognized by Code?
Regards,
Noel Tan
Topic
American Welding Society Services
/
Technical Standards & Publications
/ PLATES AS PER EN10025
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill