This is a two part question to save a lot of typeing ,because I got something in my eye and it hurts like crazy. Ok on the cap for 6g I know you can either weave or two bead. I prefer a two bead because its more consistant and seems to be stronger. I get inconsistant with the weave and some undercut at 6 oclock. Im working on both. What do most job site prefer when you go to test? Also who would I talk to for getting on as a helper? I know at that this time things are slow, but I would like to get my foot in the door. Im going to school right now, and trying to rig out a truck. I have a 71 redface sa 200 lincoln, but not sure which way to go. I normally do not have any problems with root hotpass or fill. Its cap that needs work. So I want to get on as a helper to pick up on a few things. Any suggestions?