We do robotic tig and plasma welding and feed the wire in inches per min. controlled through the analog signal board.
As for manual, that might be a bit hard to calculate since the amount of wire needed is dependent on all of the other variables. We just specify the weld size and dictate with or without filler. We do not require a specific amount of wire to be used.