Hello All
A while back there was a topic on tool boxes in shop talk so I figured I would show a couple made from 16 gage broke up with a 4' leaf brake. The first one is a top loader 34"x 20" x 12"D for my own truck bed that I am building. The lid was my first attemp at a cofin top "not easy without pan and box brake" need to adjust measurment a bit so the end pieces cutout fit back after bent. The main body is broke up in one piece so all you have to do is weld the ends in, same with the 4' under bed boxes built for customer. Those are 18" H x 15" D x 48" L with off set doors to clear tie down winches and hooks. To give you an idea on cost I have 6 hours on each 4 footer and about $125 each in materials and they still need painted.
Anyone have picture of theres and how they built them please post them up.