hey guys, just want to vent. i am the rig welder on a offshore drilling rig with 25 yers exp. our maint. crew consist of a mechanic,electrican,welder,and 2 motorman, all of these positions req. years of exp to get except for electrican. the mech. as been in the gulf for over 30 yrs. i have 25, the motorman have 15 the elec. has 18 months. this guy cant change a lite bulb without looking it up on the internet. he is 32, said he was a yeoman for 10 yrs in the navy(kinda like a secatary) also claims to be a master machinest and a master elect. the math dont add up. we have one of the most dangerous jobs in the world and this worm didnt even take a test when hired on. scared he is going to get himself or someone else killed. by the way he calls a cuttin torch a "metal disintegrater" lmao. i call him marvin martin. just another one of those guys that move here from up north and think we are just a bunch of dum rednecks