My buddy has a pinhole leak right on top of his radiator. I havent brazed for years. What would u all suggest for this repair. Very , very small hole. needle size. Brazing it with torch and brazing rod best? Thanks
Almost every radiator that I have seen has been soldered at assembly. If you put enough heat on it to braze you will probable melt some nearby joints. I have fixed a few old car radiators with a Weller soldering gun or a soldering copper. It has to be clean to be successful and that's the hard part. Good luck