TRC
Date
01-06-2009 22:14
In what application is ER70S-Cu used?
By
GRoberts
Date
01-07-2009 01:28
Is that a trade name? Unless there is something I'm missing, I don't see it as an AWS Classification (At least no in A5.18).
By
swnorris
Date
01-07-2009 14:14
Cu is the symbol for copper. Is it an electrode for copper? ERCu maybe?
By
hogan
Date
01-07-2009 14:43
Or maybe copper coated.
By
TRC
Date
01-07-2009 22:28
I looked at it again today and discovered that I left a # out, it's ER70S-3Cu- thanks for the responses- Ted
By
GRoberts
Date
01-08-2009 01:29
The ER70S-3 is an AWS classifeid carbon steel electrode. My guess is that the Cu is some manufacturer's trade name to represent either copper coating, or some amount of copper addition to the electrode.
Topic
Welding Industry
/
Technical Discussions
/ ER70S-Cu
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill