Hopefully someone with a newer D1.4 will chime in but in my 98 edition Table 5.2 it says in Note 2 that welding shall not be done when the temp is BELOW -18C, you are right there, so make a judgement call on that one....and for #9 w/ .55CE it has 200F/90C listed as the min preheat.