Hello Dave, I believe you might be able to find some pictures that you could cut/paste/copy from www.millerwelds.com or possibly www.lincolnelectric.com. I have seen copies of some of their posters that show examples of various good/bad welds. They have welds for SMAW, GMAW, and I seem to recall some for FCAW as well. The AISC website might also have some examples that you could copy, try hunting around a bit on the web, I'm pretty sure you can find quite a few examples. On the forum here, try searching under a poster by the name of "soilschick" she included some photos of some pretty bad welds that she had done some inspection on. Good luck and best regards, Allan