- - By PipeIt (**) Date 03-18-2009 19:25
Is there any data out there for the weight of rods/wire used for a given joint?

How much rod/wire for a 42" joint for example, I was asked by my boss and I didn't have an answer just a guess.

I would guess 20# for a 42" standard pipe joint.

Please advise Thanks.
Parent - - By Kix (****) Date 03-18-2009 19:50
http://www.mwsco.com/kb/kb_frameset.asp?ArticleID=111  here ya go man, this ought to help you out bunch and get you real close to what you are actually depositing.  Good luck