I am preparing to run a new PQR plate using Base Metal M270 Grade 50 Type 2 SAW process.
Per Table 4.1 (pg 77) my SAW Electrode Specification should be AWS A5.17.

Question Can I use a SAW filler metal that is per AWS A5.23 with this base metal?

I think the answer is no, I'm limited to AWS A5.17 for grade 50, and AWS A5.23 shall be used for base metal HPS 485W.  But if I am qualifiying the procedure why can't I mix and match as needed.

Thanks Chris
Parent - By HgTX (***) Date 03-26-2009 18:58
Huh?  Read two lines further down in that same box; it gives you A5.23.