I've never used GTAW to join silver but would probably try DCEN first, then AC. I'd write a weld procedure. Probably argon gas. I'd contact Harris (or another filler metal manufacture) and ask them directly what to use.
However, my first process choice would be to torch braze.
Good Luck,
Keith