According to D1.1 2006, fig 4.15... "hardened rollers 1-1/2" in diameter may be substituted for jig shoulders." My question is since it does not say SHALL, Can I build a code compliant jig with any size rollers? If not, what would be the difference, since a round surface is going to contact in only one theoretical point.