- - By griffen (*) Date 05-01-2009 11:27
What size gap and what size land do you use for a 12" butt weld with a 5/32" 5p+ ?   And also what do you have your o.c.v. set on and what gear do you run? Advice appreciated.
Parent - - By okwelder82 (***) Date 05-01-2009 13:00
I usually use a nickel land and I have 2 pieces of Banding material that you would use to band pallets together, stacked on top of each other and that gap ends up being about perfect for me.
Parent - By griffen (*) Date 05-01-2009 13:55
Thanks. Is that in 240-160?
Parent - - By dfwpipeliner (**) Date 05-01-2009 14:07
Nickel width, machine in 3rd gear, box on 40, let her burn!
Parent - - By griffen (*) Date 05-01-2009 14:58
Thanks for the reply. I'm gonna get some pipe and run some. Do you know what your o.c.v. is set at ? Are you running a 200 or 300 ?
Parent - By okwelder82 (***) Date 05-01-2009 17:33
Sorry Griffen, I forgot to put the setting on there. I have a 300D and I run 3rd gear and 40 to 50 on the box. I have the Kubota in my machine so I  can change my OCV's but Its usually around 90-91. Hope this helps.
Parent - - By dfwpipeliner (**) Date 05-02-2009 00:56
Runnin a  76' sa200,  o.c.v?  who knows? Not that schooled on the machines, just burn rods.
Parent - By griffen (*) Date 05-02-2009 01:58
hey guys mucho thanks for the info!