I think wc stands for weld cool, american optical weld cool lense.
yes the wc stands for weldcool. i have seen these lens with the WC, the AO, and even the AOWC. American Optical Weld Cool
for got to mention, it should have ither the ao, wc or aowc on the top left cornor of lens