I should think pulse would not be of much advantage to you. The pulse shoots high energy in to pudddle then backs off to back ground current you would pretty much need to feed your wire with machine percision to make a difference. We use pulse TIG but we use a auto wire feeder with it.
We have a Powcon inverter and if you dont mind the whistle sound it makes at the arc it works fine but I prefer the Hobart Cyberwave or Miller Sycrowave. If you need to be highly mobile the inverter is the only way to go. The whistle get old pretty quick though.