Fillet welding thickness limit under Section 4.25 text and Table 4.11in the D1.1 2008.
I was asked a question today that I could not definitively answer. Based upon a 3/8" plate test as in figures 4.31 or 4.32, we qualify fillet welding by the text of 4.25. Is this fillet qualified to unlimited thickness, or to an effective throat no greater than 2T? My instinct tells me to limit the fillet to 2T when the plate is under 1", but the text surrounding this really isn't clear. Perhaps I am missing something?