sir,i plan to use tig welding to weld 4130 Chromoly Alloy Steel Tubes with
O.D. =1.25 inch
Wall Thickness= 0.065 inch (1.65 mm)
could you please advice me whether i could use a TIG machine with the following specification
to weld the above tubes.the machine has an ac welding output
Make: Invertech TIG200P
Application/ Usage: TIG,PULSE TIG & MMA
Input Supply: 1Ph. 220 V, 50/60 Hz.
Rated Input (Power) Capacity KVA : 4.5
Open Circuit Voltage(V): 56
Output Current Range(A): 5-200 A
No-load Power Consumption: 40 Watts
Efficiency: 85 %
Duty Cycle: 200 Amps @ 60 %
Power Factor: 0.93
Weight (Kg) : 13.2
Dimensions (mm) : 440 x 218 x 355