Witch joint solection should I use for a pre qualified joint D1.1, Pipe,butt,no backing?
Parent - - By Lawrence (*****) Date 07-20-2009 05:15
What is the intended service of this pipe >>??

Unless you have a backing ring or back gouge and back weld that butt joint, or produce a partial penetration weld, there are no prequalified butt joint details in D1.1

D1.1 has a selection of prequalified joint details that can be used for different conditions.. drawings are right in the book.. You need to get a copy of D1.1.
Parent - - By mrwelder (*) Date 07-20-2009 12:40
I have a copy of D1.1 and API 1104. This is my first WPS for pipe. Just cant find the answers? If you can help that would be great.
Parent - By Lawrence (*****) Date 07-20-2009 13:00
Can't help if you don't answer questions.

Let's start over.

What is the purpose or intended service of the pipe?

Are you planning to make the weld full penetration from one side with an open root?

What process/es would you be using?