- - By MED Date 09-07-2004 14:30
What is the AWS B2.1 SWPS No listed in Appendix E ASME lX 2003 or 2004 for GTAW P8 without a consumable insert used.


Parent - - By jfolk (**) Date 09-07-2004 21:44
Try AWS B2.1-8-212:2001
GTAW P8/P8, as welded, primarily pipe applications. Consumable insert: not permitted.

John Folk
Parent - By MED Date 09-07-2004 21:47
Many Thanks
I purchased that SWPS about two weeks ago but do not have ASAME lX 2003 yet MED
Parent - - By JM_VRCIC (*) Date 08-05-2009 20:40
Hi, there are a couple of SWPS in the internet. You should check for them.
Parent - - By johnnyh (***) Date 08-05-2009 21:45 Edited 08-05-2009 21:49
The internet hadn't even been invented yet by Al Gore back when he asked the question.  :)
Parent - - By JM_VRCIC (*) Date 08-05-2009 23:35
?????
Anyway...
Parent - - By swsweld (****) Date 08-06-2009 02:04
Hello Juan.
I think johnnyhs' reply was in light of the thread being about five years old. Henceforth the Al Gore Internet joke.
The smiley face indicates it's all in fun.

However, I occasionally have need for SWPS and next time I will search the Internet to see if I can find what I'm looking for.

Thanks.
Parent - - By kipman (***) Date 08-06-2009 12:47
Gentlemen,
SWPS (standard WPS) are sold by AWS (see this link: https://www.awspubs.com/advanced_search_result.php?keywords=SWPS&osCsid=380344c1f6b3b1836e0cd6a23ee8ef50&x=32&y=8).  I would be very careful about using anything called a "SWPS" that you find for free on the internet.
Mankenberg
Parent - - By JM_VRCIC (*) Date 08-20-2009 21:11
I agree with you kipman, I'm just saying that they're in the internet. It's up to the person who search for them and use them the responsibility. I think this is a way to investigate some things and use them for free. Anyway, as you can see I'm not giving any link here.

Bye.
Parent - - By Lawrence (*****) Date 08-21-2009 01:08
The point is that AWS SWPS are not free, ever.

If there are pirated SWPS copies that people can download they are stealing.

There is no way to steal responsibally.
Parent - - By swsweld (****) Date 08-21-2009 02:44 Edited 08-21-2009 02:47
For the record. I have bought two SWPS's from AWS and should have worded my response more responsibly. I can see how it was misconstrued. I would not use a pirated copy but would review the content for educational purposes the same as I read the post here for educational  purposes.
Parent - By JM_VRCIC (*) Date 08-21-2009 14:31
Hi again, in fact I downloaded them but never use them, never! I downloaded them for educational purpose because nobody here knew what was a SWPS. Bye.