3.2 Inspector,
Thanks again for your interest. I just got done qualifying a bunch of ASME Sect. IX PQRs to meet the CE PED(pressure equipment directive) for a package boiler manufacturer so I am aware of BS EN ISO 15614-1:2004 +A1:2008 - Specification and qualification of welding procedures for metallic materials - Welding Procedure Test , BS EN 287-1:2004 - Qualification test of welders - Fusion Welding, BS EN ISO 5817:2007 - Welding - Fusion-welded jointws in steel, nickel, titanium and their alloys (beam welding excluded) - Quality levels for imperfections, etc. In this case AWS D1.1 will be the overriding Specification.
It's casual,
Skerfan