Hi ,
We are making pile cages of materials A36 (plain bar) to Gr.460B (rebar ) using SMAW. The procedure and welders are qualified as per BS7123:1989.
Now, I'm in ambiguity, as that BS code wont tells anything about acc. criteria. Can anyone pls solve my confusion?
Replies are appreciated.
NKumar