ocv reading 92.3 outlet plug reading 13.5 , 1/8 p5 190and 30 it's like gougeing any sugg. should i roll the rack?
By
texpipeliner
Date
09-11-2009 00:57
lower you ocv to about 89
By
Big J
Date
09-11-2009 01:04
well i had it at 87 but it would only strike arc on high idle so i mved it 2 93 , i just rebuilt every thing and trying 2 get it back where it was.
By
ibeweldingsum
Date
09-13-2009 14:35
sounds to me like you need to reseat your brushes. imho
By
KSellon
Date
09-15-2009 14:04
your low idle is set too low-- (adjust this with the solenoid linkage) Your high idle (set on governor and control rod to carb) controls the weld character.
Got pics?? I might be able to help if I had a visual on your machine linkage....
By
FixaLinc
Date
09-15-2009 23:13
Lincoln manuals IM-179G, IM-179-G1, or IM-277A
http://content.lincolnelectric.com/pdfs/products/navigator/im/obsomenu.pdf
or enter your code number at:
http://www.mylincolnelectric.com/Catalog/lecooperatorsmanualsearch.aspx
By
Big J
Date
09-17-2009 00:56
Thanks for the input got it back online. does any body know of any work going on?
By
FixaLinc
Date
09-17-2009 03:04
About I've heard about is some that government stimulus red iron going up at military bases, schools and colleges.
Topic
Welding Industry
/
General Welding Discussion
/ S.A. 200
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill