I've written procedures for it, and performed the work. However; that is at specific request of engineering as well as their specified acceptance criteria.
As a general rule of thumb, PJP's are not UT'd.
You should have a detailed procedure written by a LIII if this is done to any form of code. If you don't, then I would suggest raising that concern with the LIII you spoke of.
Regards,
Gerald