Yes, the wire feeder is CC/CV. I also use an ESAB Mobile Master wire feeder. The Lincoln rep said to run the NR-232 1/16" wire at 22V and 100ipm. I was busy with the 5/64" wire but the other welder didn't have very good results with the NR-232 wire. I didn't have time to play with it so it's possible that he didn't have it dialed in but i did run it a week ago and wasn't impressed. But after running NS3M wire nothing that I have run comes close.
I've got about a week before we do the OH weld so I might try another brand (ESAB) Just don't want to wind up sticking it out.
Thanks Lawrence and jffluxcore for the replies.