Dear Friends
During sub-assmebly stage it was noted that Main Girder Frame Web Plate exactly sitting on Butt-Joint of adjoining Face Plate( width 700mm x 32mm thk x EH36 ).
Then Reinforement was gring flush floowed by UT/MPI and found acceptable.Then Main Girder Frame installed - PJP Joint. Is it right thing to do ?
Thanks in advance