Hi Miguel,
You can test with any of the CJP joints to qualify your welders(I use a B-U4a in a 2G position in my shop[it represents the most common joint my welders will see], other shops use a B-U2a), provided you follow the guide lines in AWS D1.1:2002, Table 4.11 Welding Personnel Performance Essential Variable Changes Requiring Requalification, also see paragraph 4.22. which states:"Changes beyond the limitation of esssential variables for welders, welding operators, or tack welders shown in Table 4.11 shall require requalification."
So if "any" of the variables listed in this table have changed(omission of backing, Item #7), then a retest is necessary.
I know this code gets rather confusing when you get to reading it. That's what this forum is about, each of us look at this and try to determine what it is trying to convey to us. There are areas where we will all disagree on it's interpetation, but the "Commentary" in the back of the book helps with that. If there are paragraphs that you are confused on check in the back of the book. Annex B will give definitions to terms used also.
Hope to help,
John Wright